Cutting Surface
Top Surface (Enlarged)
Top Surface
Diameter: φ30 mm
Thickness: 0.12 mm
Number of Scans: 100
A polyimide sample was cut out using a DUV picosecond laser.
Non-thermal processing close to complete ablation was achieved, resulting in extremely clean plane of incidence, plane of reflection, and cut surfaces.、
(Surface roughness of the cut surface: Ra = 0.15 um.)
Polyimide